| BRAND |
MORTAR 1 |
MORTAR 2 |
Mortar for Insulating Bricks |
| PROPERTIES |
HM-30 |
HM-32 |
HM-34 |
HM-43 |
HM-36 |
HM-38 |
AM-30W |
AM-43W |
PM-80 |
| |
|
|
|
|
|
|
|
|
|
| PHYSICAL DATA (Typical) |
|
|
|
|
|
|
|
|
|
| Refractoriness,SK (Seger Cone) |
30 |
32 |
34 |
34 |
36 |
37 |
29 |
32 |
38 |
| Approximate. Amount Required per 1000,9" |
|
|
|
|
|
|
|
|
|
| Equivalent (Thinly Troweller Joints) kgs. |
140-180 |
140-180 |
160-200 |
160-200 |
170-210 |
165-210 |
180-230 |
160-200 |
180-270 |
| Approximate Amount of Water for Trowelling |
|
|
|
|
|
|
|
|
|
| Consistency (Dry only) Litres/50kg. |
20-25 |
20-25 |
20-25 |
|
|
|
20-25 |
20-25 |
20-25 |
| Modulus of Rupture at joints, After Drying |
|
|
|
|
|
|
|
|
|
| at 110 oC,kg/cm2 |
|
|
|
|
|
|
15-30 |
15-30 |
|
| Refractoriness Test |
|
|
|
|
|
|
|
|
|
| Mortar does not squeeze or flow from joints |
|
|
|
|
|
|
|
|
|
| when heated at, oC oC |
1400 |
1400 |
1600 |
1600 |
1600 |
1600 |
|
|
|
| |
|
|
|
|
|
|
|
|
|
| CHEMICAL ANALYSIS, % Approx. |
|
|
|
|
|
|
|
|
|
| Silica (SiO2) % |
63.5 |
56.7 |
51.2 |
50.0 |
31.4 |
27.2 |
54.1 |
47.9 |
11.4 |
| Alumina (Al2O3) % |
27.6 |
32.1 |
40.3 |
43.6 |
62.5 |
70.0 |
35.2 |
46.4 |
80.5 |
| Iron Oxide (Fe2O3) % |
2.2 |
2.0 |
2.0 |
2.0 |
1.9 |
1.2 |
2.0 |
1.9 |
1.5 |